Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 120 g/10 min @Load 3.80 kg, Temperature 230 °C |
120 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A; ASTM D1238 |
Network Polymers PC-1029 AS/P Description: Antistatic PolycarbonateInformation provided by Network Polymers Inc. |
|||
Melt Flow | 120 g/10 min @Pressure 0.655 MPa |
120 g/10 min @Pressure 95.0 psi |
Severs Efflux; Geon® ALTC 23 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series Adept E 49 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Adept E49 is a low molecular weight homopolymer dispersion resins intended for use in variety of plastisol applications and processes. It reduces scrap rates and manufacturing costs by extend.. |
|||
Melt Flow | 120 g/10 min | 120 g/10 min | (MVR) [cm³/10min]; ISO 1133 |
EMS-Grivory Grivory® CR 8 PA* Product description: Grilon CR 8 is a Copolyamide. Grilon CR 8 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesHigh shrinkageGood transparen.. |
|||
Melt Flow | 120 g/10 min | 120 g/10 min | (MVR) [cm³/10min]; ISO 1133 |
EMS-Grivory Grivory® CR 9 PA* Product description: Grilon CR 9 is a copolyamide with low melting temperature. Grilon CR 9 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesH.. |
|||
Melt Flow | 120 g/10 min @Load 1.20 kg, Temperature 300 °C |
120 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Diamond Polymers NPP 60-3301 Clear Polyester Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 120 g/10 min @Load 2.16 kg, Temperature 230 °C |
120 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem TI71200M High Crystallinity Copolymer Polypropylene Description: Highly crystalline homopolymer phase, very high molecular weight EPR phase, very high flexural modulus, reduced emissions, reduced gels.Applications: Suggested uses include compounding... |
|||
Melt Flow | 120 g/10 min @Load 5.00 kg, Temperature 275 °C |
120 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 MS Polyamide 6 - Natural Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.For uncolored parts produced by injection molding, contain including and demo.. |
|||
Melt Flow | 120 g/10 min @Load 5.00 kg, Temperature 275 °C |
120 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 Polyamide 6 - Natural Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechanical strength, rigidi.. |
|||
Melt Flow | 120 g/10 min @Load 2.16 kg, Temperature 230 °C |
120 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Carmel Olefins CAPILENE® Y 50 V Polypropylene Homopolymer CAPILENE® Y 50 V is an ultra high melt flow rate polypropylene homopolymer suitable for thin walled injection molding and as a base resin for compounds applications. The product combines high stiff.. |
|||
Melt Flow | 120 g/10 min @Load 8.40 kg, Temperature 360 °C |
120 g/10 min @Load 18.5 lb, Temperature 680 °F |
|
Performance Polymers IPS II PPL-C4050 PEKK (Polyetherketoneketone) Linear Molding Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |