Physical Properties | Metric | English | Comments |
---|---|---|---|
Carbon Dioxide Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | 23°C/0%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® CR 9 HV PA* Product description: Grilon CR 9 HV is a high viscosity copolyamide with low temperature. Grilon CR9 HV has the following features:High flexibility and toughnessGood thermoforming and orientation pr.. |
|||
Carbon Dioxide Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | 23°C/0%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® CR 9 PA* Product description: Grilon CR 9 is a copolyamide with low melting temperature. Grilon CR 9 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesH.. |
|||
Carbon Dioxide Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | 23°C/85%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® FG 40 NL nat 6018 PA6 Information provided by EMS Grivory |
|||
Carbon Dioxide Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | 23°C/85%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® FG 47 NL nat 6028 PA6 Product description: Grilon FG 47 NL natural 6028 is a modified, high viscosity Polyamide 6, which contains also slip and nucleating agents. Grilon FG 47 NL natural 6028 shows following improvements.. |
|||
Carbon Dioxide Transmission | 200 cc-mm/m²-24hr-atm | 508 cc-mil/100 in²-24hr-atm | 23°C/0%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® BM 16 nat PA* Product description: Grilon BM 16 natural is a medium viscosity multi-polyamide with a low melting point. Grilon BM 16 natural has the following features: High flexibility and toughnessVery good ori.. |