Polymer Property : Elmendorf Tear Strength TD = 2040 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 2040 g
2040 g
ISO 6383-2
EMS-Grivory Grivory® CR 8 PA*
Product description: Grilon CR 8 is a Copolyamide. Grilon CR 8 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesHigh shrinkageGood transparen..
Elmendorf Tear Strength TD 2040 g
2040 g
ISO 6383-2
EMS-Grivory Grivory® CR 9 HV PA*
Product description: Grilon CR 9 HV is a high viscosity copolyamide with low temperature. Grilon CR9 HV has the following features:High flexibility and toughnessGood thermoforming and orientation pr..
Elmendorf Tear Strength TD 2040 g
2040 g
ISO 6383-2
EMS-Grivory Grivory® CR 9 PA*
Product description: Grilon CR 9 is a copolyamide with low melting temperature. Grilon CR 9 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesH..
Elmendorf Tear Strength TD 2040 g
2040 g
ISO 6383-2
EMS-Grivory Grivory® BM 20 SBG PA*
Product description: Grilon BM 20 SBG is a lactam free multipolyamide. Grilon BM 20 SBG has the following features: Lactam freeGood transparency and glossGood flexibility and toughnessVery good ther..