Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® LC6601 BK551 Nylon 612  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Impact Modified
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® LC6601 BK551 Nylon 612  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plasticized Toughened Polyamide 612 Developed for Extrusion Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
DAM; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
DAM; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
DAM; Nominal; ISO 527-1/-2
Elongation at Yield 32 %
32 %
DAM; ISO 527-1/-2
Flexural Modulus 0.850 GPa
123 ksi
DAM; ISO 178
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
DAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
DAM; ISO 75-1/-2
Descriptive Properties Value Comments
Delivery Form Pellets
Part Marking Code >PA612-HIP<
ISO 11469
Processing Film Extrusion
Other Extrusion
Profile Extrusion
Sheet Extrusion
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PA612-HIP
PA612-HIP
ISO 1043
Special Characteristics Heat stabilised or stable to heat