Material Notes:
Description/Features:Multi-Purpose Thermoplastic ElastomerApplications:General PurposeCove BaseInteriorMarket:AutomotiveConsumer GoodsBuilding and ConstructionProcessing Method:Extrusion and MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Linear Mold Shrinkage 0.0126 cm/cm
0.0126 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 28
28
10 Sec; ASTM D2240
Tensile Strength, Yield 4.31 MPa
625 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
4.14 MPa

@Strain 300 %
600 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 375 %
375 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 34.2 kN/m
195 pli
Die C (graves), 20 in/min; ASTM D624
Thermal Properties Metric English Comments
Brittleness Temperature -62.5 °C
-80.5 °F
ASTM D746