Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | >= 0.850 GPa | >= 123 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 4441R (40404) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | >= 0.850 GPa | >= 123 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 4132B (PA14D) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates very high long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | >= 0.850 GPa | >= 123 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 4210L (EP2C30F) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | 2 mm/min; ASTM D790 |
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer
(discontinued **) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | Tangent; ASTM D790 |
Flint Hills AP7710-HS Impact Copolymer Polypropylene TPO copolymer, UL certified, and FDA compliant.Features: Structural stiffness, ultra high impact strength, and high uniform flow rate.Applications: Injection molding: automotive items and exterior e.. |
|||
Flexural Modulus | 0.850 GPa @Temperature 23.0 °C |
123 ksi @Temperature 73.4 °F |
ISO 178 |
MBA Polymers PP 2182 Post-consumer recycled polypropylene copolymer Very high melt flow rate for injection molding application. Available in standard black.Information provided by MBA Polymers. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 3325M Polypropylene Random Copolymer CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD SEALABLE CONTAINS SLIP AND ANTIBLOCK ADDITIVES APPLICATIONS: CAST FILM EXTRUSION CPP FILM FOR LAMINATE , CPP FILM FOR PACKAGINGS |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP FL003 PE LNP* LUBRICOMP* FL003 is a compound based on Polyethylene resin containing 15% PTFE. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ISO 178 |
Solvay TECHNYL® C 442 Black V PA6, DRY Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It ha.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | at 2 in/min; ASTM D790 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ASTM D790 |
Borealis Borstar® HE 6068 Natural Bimodal HDPE with very low shrinkage for Submarine and Fiber Optical Cables Borstar® HE6068 is a natural, UV-stabilized, colorable, bimodal high density (HD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar®.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ASTM D790/1 |
Borealis Borstar® HE6067 Black Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar HE6067 is a black, bimodal, co-polymer high density polyethylene (HDPE) compound produced according to the bimodal Borstar process. It is characterized by its balanced properties important .. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ISO 178 |
Borealis Daploy™ WB260HMS Polypropylene Daploy™ WB260HMS is a propylene-based, structurally isomeric polymer. Applications: cushioning and protective packaging, door liners, lightweight packaging trays, beakers and containers, microwave.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | at 2 in/min; ASTM D790 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | at 2 in/min; ASTM D790 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | at 2 in/min; ASTM D790 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ISO 178 |
Borealis RD735CF Polypropylene Random Copolymer RD735CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD735CF is recommended for food packaging, textile packaging .. |
|||
Flexural Modulus | 0.850 GPa @Temperature 23.0 °C |
123 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® FN727 BK230A Nylon 6 Zytel® FN727 BK230A is a black, impact modified, plasticizer free, very flexible polyamide 6 alloy resin having good low temperature toughness, good heat aging and good chemical resistance. Uses in.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® LC6601 BK551 Nylon 612
(Unverified Data**) Plasticized Toughened Polyamide 612 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 0.850 GPa @Temperature 23.0 °C |
123 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® ST811HS BK038 Nylon 6
(Unverified Data**) Zytel® ST811HS BK038 is a flexible, non-plasticized, black Super Tough nylon 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores an.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | 1% secant; ASTM D790 |
Braskem CP 195 Injection Molding Polypropylene Description: CP 195 is a very high melt flow rate heterophasic copolymer developed for high speed injection moulding machines and high productivity thin-walled injection moulded parts. The product f.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | SAE J949 |
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness) AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ASTM D790 |
Carmel Olefins CAPILENE® TR 50 Polypropylene Impact Copolymer Description: CAPILENE® TR 50 is a medium melt flow rate heterophasic copolymer with very high impact strength, even at low temperature, designed for injection molding. This grade combines good pr.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ASTM D790 |
Carmel Olefins CAPILENE® TT 75 AV Polypropylene Impact Copolymer Description: CAPILENE® TT 75 AV is a nucleated, controlled rheology heterophasic copolymer designed for injection molding. It is characterized by excellent impact strength, even at low temperatur.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ASTM D790 |
Carmel Olefins CAPILENE® TU 75 AV Polypropylene Impact Copolymer Description: CAPILENE® TU 75 AV is a high melt flow rate, controlled rheology heterophasic copolymer with very high impact strength, even at low temperature. It contains antistatic and nucleating.. |
|||
Flexural Modulus | 0.850 GPa @Temperature 93.0 °C |
123 ksi @Temperature 199 °F |
ASTM Test |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Conditioned) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2607-UV9 HDPE Injection Molding Resin
(discontinued **) Features: Excellent stiffness, good impact resistance, low warpage.Applications: Roll-out carts.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers DEXPRO® R120 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R120 is a reactor-grade thermoplastic elastomeric olefin resin with a good balance of impact performance, stiffness, and paintability. Applications: Painted bumper fasciasInfor.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ASTM D790/1 |
Borealis Borstar® HE6062 HDPE Black Jacketing Compound Borstar HE6062 is a black, bimodal co-polymer high density polyethylene (HDPE) compound produced using the Borealis Borstar process. It is characterized by balanced properties important in jacketin.. |
|||
Flexural Modulus | 0.850 GPa | 123 ksi | ASTM D790 |
Borealis Borstar® HE6063 Natural Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar HE6063 is a natural, colorable, bimodal, high-density polyethylene compound, produced using the Borstar process, for jacketing of power and telecommunications cables. It is characterized by.. |