Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® 74G33J NC010 Nylon 66  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® 74G33J NC010 Nylon 66  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
33% Glass Reinforced Polyamide 66 + Polyamide 6 Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Modulus 6.00 GPa
870 ksi
50%RH; ISO 527-1/-2
10.0 GPa
1450 ksi
DAM; ISO 527-1/-2
Charpy Impact Unnotched 8.50 J/cm²
40.4 ft-lb/in²
DAM; ISO 179/1eU
10.0 J/cm²
47.6 ft-lb/in²
50%RH; ISO 179/1eU
6.50 J/cm²

@Temperature -30.0 °C
30.9 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eU
7.00 J/cm²

@Temperature -30.0 °C
33.3 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
DAM; ISO 179/1eA
1.80 J/cm²
8.57 ft-lb/in²
50%RH; ISO 179/1eA
1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eA