Loctite® Ultra Grey® 5999 Flange Sealant

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Loctite
Trade Name Ultra Grey®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® Ultra Grey® 5999 Flange Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Silicone GasketingLoctite® Silicone Gasketing materials include unique products with excellent resistance, formulations for high operating temperatures, and UV-curing formulations for cure-in-place production requirements. Silicone gasketing products are best suited for large gap applications and stamped metal assemblies where flexing occurs.Loctite® 5999 Form-in-place Heavy Body RTV Silicone Ultra Grey® Flange SealantHigh modulus for rigid flange assemblies. Heavy body provides instant seal. Excellent oil, transmission fluid, gear oil, and water/glycol resistance. Non-corrosive. Low odor. Low volatility. Grey. Cure Type: Moisture Typical Use: Oil/water resistant, instant seal
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength, Ultimate 3.45 MPa
500 psi
Elongation at Break 175 %
175 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 10.0 min
0.167 hour
Tack-free
1440 min
24.0 hour
Full Cure; Varies with substrates
Descriptive Properties Value Comments
Color Grey
Extrusion Rate 105 g/min
Gap Fill 0.24 in.