Material Notes:
Data provided by DuPont Packaging Polymers.A machine direction oriented nylon type 6,6 film. Many of the properties of nylon 6,6 film are improved upon orientation, but particularly the overall toughness and gas permeability. Provides excellent qualities to the converter which make it an ideal film for printing and laminating. Its barrier properties and stiffness make it an excellent choice for a variety of packaging end uses such as snacks, processed meat, cheese, condiments.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
Moisture Vapor Transmission 2.18 cc-mm/m²-24hr-atm
5.54 cc-mil/100 in²-24hr-atm
ASTM E398-70
Water Vapor Transmission 145 g/m²/day
9.34 g/100 in²/day
ASTM E398-70
Oxygen Transmission 0.590 cc-mm/m²-24hr-atm
1.50 cc-mil/100 in²-24hr-atm
or 39 cc/m²-24hr-atm for the film at 23°C, 0% RH. ASTM D1434-66
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 50 %
50 %
ASTM D882
Film Elongation at Break, TD 250 %
250 %
ASTM D882
Secant Modulus, MD 2.26 GPa
328 ksi
ASTM D882
Secant Modulus, TD 2.26 GPa
328 ksi
ASTM D882
Elmendorf Tear Strength, MD 3.00 g/micron
76.2 g/mil
ASTM D1922-67
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
ASTM D1922-67
Film Tensile Strength at Break, MD 240 MPa
34800 psi
ASTM D882
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
Gloss 150 %
150 %