Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp WB006 PBT (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Bead Filled
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp WB006 PBT (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* WB006 is a compound based on Polybutylene Terephalate resin containing Glass Bead.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.020 cm/cm
0.020 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.0 MPa
6380 psi
5 mm/min; ISO 527
Elongation at Break 4.0 %
4.0 %
5 mm/min; ISO 527
Flexural Yield Strength 81.0 MPa
11700 psi
2 mm/min; ISO 178
Flexural Modulus 3.30 GPa
479 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
181 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D 257
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D 257
Users viewing this material also viewed the following: