Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 4.99 g/micron
127 g/mil
ASTM D1922
Westlake EMAC® SP2242 Specialty Copolymer  (discontinued **)
EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo..
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
ASTM D1922
NOVA Chemicals Sclair® 14B3 Butene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer.
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
ASTM D1922-67
DuPont™ Dartek® O-401 Nylon 6,6 Oriented Film, 15 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A machine direction oriented nylon type 6,6 film. Many of the properties of nylon 6,6 film are improved upon orientation, but particularly the overall tou..
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
Dow LDPE 133A Low Density Polyethylene, Blown Film Grade
DOW LDPE 133A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of antib..
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
Dow LDPE 135A Low Density Polyethylene, Blown Film Grade
DOW LDPE 135A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of slip ..
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
Dow LDPE 132I Low Density Polyethylene, Blown Film Grade
DOW LDPE 132I is a barefoot resin for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It complies with U.S. FDA re..
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
ASTM-D1922
Braskem TN7006 LDPE Blown Film Extrusion Polyethylene
TN7006 is a low-density polyethylene (LDPE) specially developed for coextruded films and lamination. The resin presents a great combination of mechanical, optical, and stiffness properties. TN7006 h..
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
ASTM-D1922
Braskem TS7006 LDPE Blown Film Extrusion Polyethylene
TS7006 is a low-density polyethylene (LDPE) specially developed for coextruded films and lamination. The resin presents a combination of mechanical, optical, and stiffness properties. TS7006 has a l..
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
ISO 6283-2
Carmel Olefins IPETHENE® 100 Low Density Polyethylene
IPETHENE® 100 is a low density polyethylene extrusion grade. It exhibits good impact and puncture resistance, good processability and good ESCR. APPLICATIONS IPETHENE® 100 is used for production..
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
ISO 6283-2
Carmel Olefins IPETHENE® 111 Low Density Polyethylene
IPETHENE® 111 is a low density polyethylene extrusion grade, contains no additives. It exhibits a good balance between mechanical and optical properties. APPLICATIONS IPETHENE® 111 is used to pr..
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
ISO 6283-2
Carmel Olefins IPETHENE® 113 Low Density Polyethylene
IPETHENE® 113 is a general purpose low density polyethylene film extrusion grade. It contains medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between me..
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
ISO 6283-2
Carmel Olefins IPETHENE® 320 Low Density Polyethylene
IPETHENE® 320 is a general purpose low density polyethylene film extrusion grade, containing no additives. It exhibits good mechanical and optical properties. APPLICATIONS IPETHENE® 320 is mainl..
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
ISO 6283-2
Carmel Olefins IPETHENE® 322 Low Density Polyethylene
IPETHENE® 322 is a general purpose low density polyethylene film extrusion grade. It contains a medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between ..
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
ISO 6283-2
Carmel Olefins IPETHENE® 323 Low Density Polyethylene
IPETHENE® 323 is a general purpose low density polyethylene film extrusion grade. It contains a high level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between me..
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
ISO 6283-2
Carmel Olefins IPETHENE® 4203 Low Density Polyethylene
IPETHENE® 4203 is a low density polyethylene extrusion grade. It exhibits good impact and puncture resistance, very good bubble stability in thick-gauge blown film processing, and excellent ESCR. ..
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
ASTM D1922
NOVA Chemicals Sclair® 14B1 Butene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer.
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
ASTM D1922-67
DuPont™ Dartek® UF-410 Nylon 6,6 Oriented Film, 15 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A monoaxially oriented nylon 6,6 film with good "slip" characteristics, which ensure excellent machinability/runnability even at high relative humidity con..
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
ASTM D1922
SABIC HP2022 Series Low Density Polyethylene for Blown Film
Product Description: HP2022 series resins are Low Density Polyethylene grades suitable for general purpose packaging. They exhibit better draw down, good optical and mechanical properties.HP2022N:..