Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 240 MPa
34800 psi
ASTM D882
DuPont™ Dartek® O-401 Nylon 6,6 Oriented Film, 15 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A machine direction oriented nylon type 6,6 film. Many of the properties of nylon 6,6 film are improved upon orientation, but particularly the overall tou..
Film Tensile Strength at Break, MD 240 MPa
34800 psi
ASTM D882
DuPont™ Dartek® UF-410 Nylon 6,6 Oriented Film, 15 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A monoaxially oriented nylon 6,6 film with good "slip" characteristics, which ensure excellent machinability/runnability even at high relative humidity con..