Dow Corning XIAMETER® PMCPPMX-200 100CS Silicone Fluid

Category Fluid
Manufacturer Dow Corning
Trade Name XIAMETER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning XIAMETER® PMCPPMX-200 100CS Silicone Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is chemically equivalent to DOW CORNING® 200 FLUID 100CS. 100% active, 100 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc

@Temperature 25.0 °C
0.960 g/cc

@Temperature 77.0 °F
Viscosity Measure 100 cSt
100 cSt
Kinetic/Kinematic
Surface Tension 20.9 dynes/cm
20.9 dynes/cm
Thermal Properties Metric English Comments
Thermal Conductivity 0.155 W/m-K
1.08 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Pour Point -65.0 °C
-85.0 °F
Flash Point >= 100 °C
>= 212 °F
Closed Cup
>= 326 °C
>= 619 °F
Open Cup
Optical Properties Metric English Comments
Refractive Index 1.403
1.403
Descriptive Properties Value Comments
Hydrophobic Yes