Polymer Property : Viscosity Measure = 100 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Measure 100 cSt
100 cSt
Shin-Etsu Silicones KF-7312J Fluid
Information Provided by Shin-Etsu Silicones of America, Inc.
Viscosity Measure 100 cSt
100 cSt
Kinetic/Kinematic
Dow Corning Q7-9120 Silicone Fluid, 100 CST
Polydimethylsiloxane fluid, excipient for pharmaceutical and cosmetic applications.Information provided by Dow Corning
Viscosity Measure 100 cSt
100 cSt
Kinetic/Kinematic
Dow Corning XIAMETER® PMCPPMX-0210 Silicone Fluid 100CS
Is chemically equivalent to DOW CORNING® 210H FLUID 100CS. This product is a heat stabilized polydimethlysiloxane, used for heat transfer.Information provided by Dow Corning
Viscosity Measure 100 cSt
100 cSt
Kinetic/Kinematic
Dow Corning XIAMETER® PMCPPMX-200 100CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 100CS. 100% active, 100 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
Viscosity Measure 100 cSt
100 cSt
Kinetic/Kinematic
Dow Corning 360 Medical Fluid, 100 CST.
Colorless and odorless polydimethysiloxane fluid for lubrication and siliconization of glass, metals, plastics and rubber in medical applications.Information provided by Dow Corning
Viscosity Measure 100 - 6000 cSt
100 - 6000 cSt
Kinetic/Kinematic
Dow Corning 5225C Formulation Aid
A 10% dispersion of high molecular weight silicone polyether in cyclopentasiloxane fluid for use in skincare, suncare, hair care, color cosmetic, and antiperspirant / deodorant applications. INCI Na..