Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.155 W/m-K | 1.08 BTU-in/hr-ft²-°F | |
Styron Magnum™ 344HP ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Thermal Conductivity | 0.155 W/m-K | 1.08 BTU-in/hr-ft²-°F | Melt |
Covestro Bayblend® T88-2N Polycarbonate + ABS, 10% Glass Filled Injection molding grade10 % glass fiber filledtensile modulus = 3900 MPaVicat/B 120 temperature = 131 °CPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
|
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 1200 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 1400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 142 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 200 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 75 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K | 1.08 BTU-in/hr-ft²-°F | |
Dow Corning XIAMETER® PMCPPMX-200 100CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 100CS. 100% active, 100 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 300 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 500 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 750 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 900 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 92 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |