Dow AFFINITY™ PT 1409 Polyolefin Plastomer (POP)

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Dow Chemical
Trade Name AFFINITY™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow AFFINITY™ PT 1409 Polyolefin Plastomer (POP).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AFFINITY™ PT 1409 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies from Dow Plastics. Resin blended with 20 wt% LDPE to improve extrusion coating performance.Information provided by Dow
Physical Properties Metric English Comments
Density 0.911 g/cc
0.0329 lb/in³
ASTM D792
Thickness >= 6.35 microns
>= 0.250 mil
Coating Thickness; Extrusion Coating Processability; Dow Method
Melt Index of Compound 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Neck In 11.4 cm
4.49 in
610°F and 1.0 mil; Extrusion Coating Processability; Dow Method
Coating Weight >= 6.08 g/m²
>= 3.80 lb/ream
Extrusion Coating Processability; Dow Method
Thermal Properties Metric English Comments
Melting Point 108 °C
226 °F
Dow Method (DSC)
Vicat Softening Point 91.0 °C
196 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 288 - 321 °C
550 - 610 °F
Extrusion Coating Processability