Physical Properties Metric English Comments
Neck In 11.4 cm
4.49 in
610°F and 1.0 mil; Extrusion Coating Processability; Dow Method
Dow AFFINITY™ PT 1409 Polyolefin Plastomer (POP)
AFFINITY™ PT 1409 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies from Dow Plastics. Resin blended with 20 wt% LDPE to improve extrusion coating performance.Information provided b..