Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 108 °C | 226 °F | Internal method |
Polimeri Europa Riblene® GP 20 Low Density Polyethylene - Coating Grade Riblene GP 20 is a high fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GP 20 is suitable for coating applications where low neck-in and high draw-down are key factors. F.. |
|||
Melting Point | 108 °C | 226 °F | Internal method |
Polimeri Europa Riblene® GP 26 Low Density Polyethylene - Coating Grade Riblene GP 26 is a high fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GP 26 is suitable for coating applications where low neck-in and high draw-down are key factors. F.. |
|||
Melting Point | 108 °C | 226 °F | Internal method |
Polimeri Europa Riblene® MQ 10 Low Density Polyethylene - Injection Molding Riblene MQ 10 is a good fluidity low density polyethylene resin (LDPE).Parts made with Riblene MQ 10 are characterized by a high flexibility.Main Applications: Riblene MQ 10 is suitable for injecti.. |
|||
Melting Point | 108 °C | 226 °F | Internal method |
Polimeri Europa Riblene® MQ 10 R Low Density Polyethylene - Injection Molding Riblene MQ 10 R is a good fluidity low density polyethylene resin (LDPE).Parts made with Riblene MQ 10 R are characterized by a high flexibility.Main Applications: Riblene MQ 10 R is suitable for i.. |
|||
Melting Point | 108 °C | 226 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 146.NH Cast Film Resin
(discontinued **) LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical |
|||
Melting Point | 108 °C | 226 °F | Freezing Point, DSC; ASTM D3418 |
DuPont Bynel® 41E689 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Melting Point | 108 °C | 226 °F | |
LyondellBasell Lupolen® 2012 D SW 413 LDPE Cable sheathingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 108 - 124 °C | 226 - 255 °F | ASTM D127 |
IRPC Polimaxx Polene PE200N Polypropylene Wax APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING |
|||
Melting Point | 108 - 124 °C | 226 - 255 °F | ASTM D127 |
IRPC Polimaxx Polene PE250N Polypropylene Wax APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING |
|||
Melting Point | 108 °C | 226 °F | |
LyondellBasell Lupolen® 1842 D SW 413 LDPE Cable sheathingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 108 °C | 226 °F | |
LyondellBasell Lupolen® 1800 S LDPE, Injection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 108 °C | 226 °F | |
LyondellBasell Lupolen® 1804 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 108 °C | 226 °F | |
LyondellBasell Lupolen® 1810 D LDPE Blow moldings, sheet, profile, film.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 108 °C | 226 °F | |
LyondellBasell Lupolen® 1810 E LDPE Blow moldingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 108 °C | 226 °F | |
LyondellBasell Lupolen® 1812 D LDPE Insulation for cableData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 108 °C | 226 °F | |
LyondellBasell Lupolen® 1840 H LDPE Blow moldings, injection moldings, film.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 108 °C | 226 °F | Upon Melting via DSC/ASTM D3418 |
DuPont 20 Series DPE 20 Specialty Polyethylene Resin DuPont 20 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding flex.. |
|||
Melting Point | 108 °C | 226 °F | ISO 11357 |
Total LDPE 1070 MN 18 C Low Density Polyethylene - Injection Molding and Compounding LDPE 1070 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant. Grade adapted to the production of flexible parts with a high production rate.Applicat.. |
|||
Melting Point | 108 °C | 227 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 316.19 High Clarity, High Impact Film Resin LD 316.19 has improved impact strength and heat sealability versus homopolymer clarity film resins. Applications include frozen and other food packaging, as well as profile extrusion.Information pr.. |
|||
Melting Point | 108 °C | 226 °F | Dow Method (DSC) |
Dow 621I Low Density Polyethylene (LDPE) Specialty resin designed for high melt strength applications Provides excellent bubble stability Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
Melting Point | 108 °C | 226 °F | Dow Method (DSC) |
Dow 662I Low Density Polyethylene Resin Blown Film Resin designed for enhanced bubble stability High melt strength Optimum gauge range: 1.5 - 5.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
Melting Point | 108 °C | 226 °F | Dow Method (DSC) |
Dow AFFINITY™ PT 1409 Polyolefin Plastomer (POP) AFFINITY™ PT 1409 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies from Dow Plastics. Resin blended with 20 wt% LDPE to improve extrusion coating performance.Information provided b.. |
|||
Melting Point | 108 °C | 226 °F | ISO 11357 |
Carmel Olefins IPETHENE® 670 Low Density Polyethylene IPETHENE® 670 is a low density polyethylene extrusion coating and lamination grade. This grade can be processed at high coating temperatures and coating speeds. It exhibits low neck-in and stable w.. |
|||
Melting Point | 108 °C | 226 °F | ASTM D3418, ISO 3146 |
DuPont™ Fusabond® M603 Polymer Modifier Fusabond® M603 Resin is a random ethylene copolymer, incorporating a monomer which is classified as being a maleic anhydride equivalent for application uses.Fusabond® M603 is used in a variety of .. |
|||
Melting Point | 108 °C | 226 °F | Exxon Method |
ExxonMobil Escorene® LD-316 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 1.9% vinyl acetate copolymer, high clarity film resin. Film made from LD-316 offers improved impact strength and heat sealability versus homopoly.. |