Information provided by Domo.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ISO 1183
Melt Flow 33 g/10 min
33 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Modulus 1.60 GPa
232 ksi
ISO 527-2
Izod Impact, Notched (ISO) 1.10 kJ/m²

@Temperature -30.0 °C
0.523 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
2.20 kJ/m²

@Temperature 23.0 °C
1.05 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
DSC; ISO 3146
Vicat Softening Point 93.0 °C
199 °F
B50 (50N); ISO 306
152 °C
306 °F
A50 (10N); ISO 306