Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 1.10 kJ/m²

@Temperature -40.0 °C
0.523 ft-lb/in²

@Temperature -40.0 °F
ISO 180
LyondellBasell Hostacomâ„¢ SP98F/94 Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ SP98F/94 Black medium melt flow, 2,300 MPa flexural modulus, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of stiffness, impact ..
Izod Impact, Notched (ISO) 1.10 kJ/m²

@Temperature -30.0 °C
0.523 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Domo 1040SC Polypropylene Homopolymer
Information provided by Domo.