| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
| Melt Flow | 0.90 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.90 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 122 | 122 | ASTM D785 |
| Tensile Strength, Yield | 80.6 MPa | 11700 psi | ASTM D638 |
| Flexural Modulus | 3.576 GPa | 518.7 ksi | ASTM D790 |
| Izod Impact, Notched | 0.107 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
0.200 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flammability, UL94 | HB @Thickness 1.59 mm |
HB @Thickness 0.0625 in |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90 % | 90 % | transparent; thickness not quantified |