Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.576 GPa | 518.7 ksi | ASTM D790 |
Diamond Polymers SAN 250 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |