Material Notes:
Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, components can be plated using conventional plating schemes to allow for assembly and integration operations. The CPS fabrication process provides a material that has a unique combination of physical properties: a compatible CTE, high thermal conductivity, light weight, and tight dimensional tolerance without machining (i.e. net-shape).Information provided by Ceramic Process Systems.
Physical Properties Metric English Comments
Density 2.99 g/cc
0.108 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 217.5 GPa
31550 ksi
Young's Modulus
Poissons Ratio 0.154
0.154
Fracture Toughness 11.67 MPa-m½
10.62 ksi-in½
Shear Modulus 94.2 GPa
13700 ksi
Thermal Properties Metric English Comments
CTE, linear 6.60 µm/m-°C

@Temperature 30.0 °C
3.67 µin/in-°F

@Temperature 86.0 °F
9.00 µm/m-°C

@Temperature 250 °C
5.00 µin/in-°F

@Temperature 482 °F
Specific Heat Capacity 0.741 J/g-°C
0.177 BTU/lb-°F
Thermal Conductivity 180 W/m-K
1250 BTU-in/hr-ft²-°F