Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 81.0 MPa | 11700 psi | ASTM D638 |
NYCOA 1047 PA 6 UL rated heat stabilized grade for applications greater than 100 deg. CInformation provided by NYCOA, Inc. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | SABIC - Japan Method |
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | SABIC - Japan Method |
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | SABIC - Japan Method |
SABIC Innovative Plastics Lexan® LGN1500 PC (Asia Pacific) |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Faradex ZX93134 PPE+PS (Europe-Africa-Middle East) LNP* Faradex* ZX93134 is a compound based on PPE+PS Blend resin containing Stainless Steel Fiber and Glass Fiber. Added features include: Electrically Conductive, EMI/RFI Shielding.This data was su.. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | ISO 527 |
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific) LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli.. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp DFP22H PC LNP* Lubricomp* DFP22H is a compound based on Polycarbonate containing Glass Fiber and PTFE. Characteristics of this grade are: Internally Lubricated and Healthcare.This data was supplied by SABIC.. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | ISO 527 |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded
( AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | ASTM D638 |
NOVA Chemicals Dylark® 480P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | ISO 527 |
SABIC Innovative Plastics LNP Lubricomp DFI12E PC LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli.. |
|||
Tensile Strength, Yield | 80.4 MPa @Thickness 3.20 mm |
11700 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUMID GP1000B(W) PA66, General Purpose, Low Viscosity Feature: Injection Molding, PA66, General Purpose, Low ViscosityApplication: Buckles, Chair NobCAS No. 32131-17-2Information provided by LG Chemical |
|||
Tensile Strength, Yield | 81.0 MPa @Temperature 22.0 °C |
11700 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0170 Unsaturated Polyester UP SMC 0170 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Tensile Strength, Yield | 80.7 MPa | 11700 psi | ASTM D638 |
Global XNY-577 20% Reinforced Polycarbonate/Polyester Alloy Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RX05487 PA 66 LNP* LUBRICOMP* RX05487 is a compound based on Nylon 66 containing 10% Aramid Fiber, 10% Lubricant. Added features of this material are: Low Warpage, Wear Resistant. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF002 PC LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF002H PC LNP THERMOCOMP* DF002H is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added feature includes: Healthcare. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MF006A PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF006A is a compound based on Polypropylene resin containing Glass Fiber. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MF006SXP PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF006SXP is a compound based on Polypropylene resin containing Glass Fiber. Added features include: Chemically Coupled. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | ISO 527 type 1 A |
Solvay TECHNYL® A 216 PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: TECHNYL ® A 216 offers all of the primary propert.. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | ISO 527 type 1 A |
Solvay TECHNYL® A 216 NATURAL FA PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 Natural FA offers all of the primary properties of unreinf.. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico.. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | |
Hexcel® HexPly® EH04 Epoxy Resin System HexPly® EH04 is a modified epoxy resin system specifically designed for bladder molding or sheet wrap tube applications. Unique chemistry provides full cured parts in only 3 minutes at 138°C.Appli.. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | |
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix HexPly® M36 is a high performance 180ºC cure matrix developed for aerospace and industrial markets. It can be used in a variety of production techniques (Resin Film Infusion (RFI), prepreg and sem.. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | dry; ISO 527-1/-2 |
DSM Novamid® 3010N 5-SL4-3X NAT PA66 FR Low Viscosity, Molding Release, 30% Glass Reinforced |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | chs 0.2 in/min; ASTM D638 |
Diamond Polymers NPP30-0800 GF40 40% Glass Filled Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 80.6 MPa | 11700 psi | ASTM D638 |
Diamond Polymers SAN 250 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | ISO 527-2 |
Cathay PA56 Renewable Engineering Polyamide, DAM Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Tensile Strength, Yield | 81.0 MPa | 11700 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000A PC (Europe-Africa-Middle East) LNP* Thermocomp* Lexan_LGN2000A compound is a 20% glass reinforced PC, high flow. UL rated V-0. Consumer Electronics applications. |
|||
Tensile Strength, Yield | 80.7 MPa | 11700 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® ATH-30GF/000 Acetal-Homopolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |