Diamond Polymers DIAMALOY FR530 PC/PBT Alloy, 30% Glass Filled Flame Retardant

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY FR530 PC/PBT Alloy, 30% Glass Filled Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D955
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 265 °C
25 g/10 min

@Load 4.76 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 114 MPa
16500 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 7.59 GPa
1100 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.850 J/cm

@Thickness 3.17 mm
1.59 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 5VA

@Thickness 1.59 mm
5VA

@Thickness 0.0625 in
5VA

@Thickness 3.17 mm
5VA

@Thickness 0.125 in