Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.59 GPa | 1100 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP JF004E PES (Asia Pacific) LNP* Thermocomp* JF004E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 7.59 GPa | 1100 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP JF004EXP PES LNP* THERMOCOMP* JF004EXP is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 7.59 GPa | 1100 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP JF004EXP PES (Asia Pacific) LNP* Thermocomp* JF004EXP is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 7.59 GPa | 1100 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP BF004 SAN LNP* THERMOCOMP* BF004 is a compound based on SAN resin containing 20% Glass Fiber. |
|||
Flexural Modulus | 7.59 GPa | 1100 ksi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers DIAMALOY FR530 PC/PBT Alloy, 30% Glass Filled Flame Retardant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 7.59 GPa | 1100 ksi | ASTM Test |
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Dry) Ultramid 1703-2 BK ND3007 is a 25% glass reinforced, heat stabilized injection molding nylon 6/6. |
|||
Flexural Modulus | 7.59 GPa | 1100 ksi | ASTM Test |
BASF Nypel® 2367G HS BK 15/25% Glass/Mineral Filled PA6 (Dry) Nypel 2367G HS BK-4 is a black pigmented, heat stabilized, 40% mineral and glass fiber reinforced injection molding compound based on recycled PA6 feedstocks. It possesses a balance of engineering .. |
|||
Flexural Modulus | 7.59 GPa | 1100 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP JF004E PES LNP* THERMOCOMP* JF004E is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. |