Diamond Polymers ABS 9950 Injection Molding Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers ABS 9950 Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 1.3 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.3 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.0 MPa
6240 psi
chs 2 in/min; ASTM D638
Elongation at Yield 5.0 %
5.0 %
chs 2.0 in/min; ASTM D638
Tensile Modulus 0.778 GPa
113 ksi
chs 2.0 in/min; ASTM D638
Flexural Strength 63.0 MPa

@Thickness 3.17 mm
9140 psi

@Thickness 0.125 in
chs 0.05 in/min; ASTM D790
Flexural Modulus 2.005 GPa

@Thickness 3.17 mm
290.8 ksi

@Thickness 0.125 in
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 4.00 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
7.49 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 105 °C

@Load 1.00 kg,
Thickness 3.17 mm
221 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525