Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Crastin® S600F40 BK851 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer DuPont Performance Polymers
Trade Name Crastin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Crastin® S600F40 BK851 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 BK851 is an unreinforced lubricated low viscosity black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Melt Flow 32.9 g/10 min

@Load 2.16 kg,
Temperature 250 °C
32.9 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.0 MPa
8410 psi
ISO 527-1/-2
Elongation at Break 20 %
20 %
Nominal; ISO 527-1/-2
Elongation at Yield 6.0 %
6.0 %
ISO 527-1/-2
Tensile Modulus 2.60 GPa
377 ksi
ISO 527-1/-2
Flexural Strength 85.0 MPa
12300 psi
ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10
Flame Spread 28 mm/min

@Thickness 1.00 mm
1.1 in/min

@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Descriptive Properties Value Comments
Part Marking Code >PBT<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PBT