Polymer Property : Flexural Modulus = 2.005 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.005 GPa

@Thickness 3.17 mm
290.8 ksi

@Thickness 0.125 in
tangent; chs 0.05 in/min; ASTM D790
Diamond Polymers ABS 9950 Injection Molding Grade
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.