Reltek BONDiT™ A-53 Bonding Agent, Adhesive and Primer

Category Polymer , Adhesive
Manufacturer Reltek LLC
Trade Name BONDiT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reltek BONDiT™ A-53 Bonding Agent, Adhesive and Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A-53 is an adhesion promoter and primer for cationic UV cure systems. It is a broad-based adhesion promoter and primer that will not poison cationic cure coatings and adhesives. Ambient cure 60 min or accellerated thermal cure. Water white color.Information provided by Reltek LLC
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Descriptive Properties Value Comments
Color Clear