Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Cond)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Cond).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temperatures Excellent resistance to wear and low friction Outstanding flow for easy processing and exceptional design freedomStanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical propertiesKey Applications: Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensionersE&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliancesInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.76 g/cc
0.0636 lb/in³
(DAM); ISO 1183
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
DAM; ISO 294-4
0.0070 cm/cm
0.0070 in/in
DAM; ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 170 MPa
24700 psi
ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
ISO 527-1/-2
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-1/-2
Charpy Impact Unnotched 8.00 J/cm²

@Temperature -30.0 °C
38.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.90 J/cm²

@Temperature -30.0 °C
9.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
10°C/min (DAM); ISO 11357-1/-3
Descriptive Properties Value Comments
Injection molding Yes
With Fillers Yes
Users viewing this material also viewed the following: