Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 GF 30 HI PA66, 30% glass fibre, improved strength FeaturesPA 66 for injection moulding, chemically strengthened with 30% glass fibre and with the content of thermoplastic kaoutchouc. Application: impacted mouldings and mouldings with high strength .. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1192C PC Copolymer High flow, polycarbonate siloxane copolymer resin. Notched izod ductile to -20C ductility. Enhanced processability compared to standard PC resins. Available in a range of transparent colors.
US .. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6
(Unverified Data**) Zytel® 73G45 BK263 is a 45% glass fiber reinforced, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6
(Unverified Data**) Zytel® 73G50HSLA BK416 is a 50% glass fiber reinforced, heat stabilized, lubricated, polyamide 6 resin for injection molding. It has an excellent surface appearance and gloss.Information provided .. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -40.0 °C |
9.04 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eA |
Kuraray Genestarâ„¢ N1001D-U83/02 Nylon Standard unreinforced extrusion grade. Main Features:Outstanding fuel barrierHeat resistanceExample of applications:Multi-layered fuel tube |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eA |
Lanxess Pocan® DP C 1502 000000 PBT + PC PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1A |
Gromax BTE70-DN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Ultem ATX100 PEI (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend. UL94 HB Listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® M201AS ABS Novodur M201AS is a medium impact, high gloss injection molding grade with improved chemical resistanceInformation provided by Styrolution |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179/1eA |
Styron MAGNUMâ„¢ 8391 Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 8391 ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass continuous process) ABS technology of Styron ensures an ABS resin that .. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Terluran® GP-25 ABS Terluran GP-25 is an easy-flow, general purpose injection molding grade with high resistance to impact and heat distortion; intended for a wide range of applications, particularly in the housings se.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Suzhou Hipro Polymers Hiprolon® 200 MC HLS G30 Nylon 1010, 30% glass fiber filled Hiprolon® 200 MC HLS G30 is a polyamide 10.10 compound reinforced with 30% chopped glass fiber for injection molding; features high dimension stability, chemical resistance, impact resistance, lo.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polyram Polytron P40B07 Polypropylene, 40% Long Glass Fiber, UV Stabilized A chemically coupled 40% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Novamid® 1013G30 1 NA PA6-GF30 30% Glass Reinforced, Injection Molding |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Novamid® 1013GH30 1 NA/BK701 PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TW241F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -40.0 °C |
9.04 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eA |
Eurotec® Tecomid® NA40 GR50 NL PA 6.6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Dry, 60% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, Conditioned Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Novamid® MC112LG55 C10 PA6-GF55 55% Glass Reinforced |