Material Notes:
Thermal conductive material, Flame Retardant, Heat Stabilized
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
dry; ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
Sim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.0030 cm/cm
0.0030 in/in
Sim. To ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.0 MPa
7980 psi
dry; ISO 527-1/-2
Elongation at Break 0.60 %
0.60 %
dry; ISO 527-1/-2
Tensile Modulus 11.0 GPa
1600 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
dry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 25.0 µm/m-°C
13.9 µin/in-°F
dry; ISO 11359-1/-2
Thermal Conductivity 1.00 W/m-K
6.94 BTU-in/hr-ft²-°F
through plane; ASTM E1461
5.00 W/m-K
34.7 BTU-in/hr-ft²-°F
in plane; ASTM E1461
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
dry; IEC 60695-11-10
V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
dry; IEC 60695-11-10
Electrical Properties Metric English Comments
Comparative Tracking Index 575 V
575 V
dry; IEC 60112