Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1100-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-10 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1100V-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-10 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1200-15 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-15 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-20 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1200H-20 Polyester SMC Premi-Glas® 1200H-20 is a 20% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94HB flame rec.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1205 Glass Reinforced SMC Description: Premi-Glas® 1205 is a glass reinforced thermoset Sheet Molding Compound formulated for residential door skins and similar construction applications. Key features and benefits: Excellen.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1240-20 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-20 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 1268 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1268 is a fiberglass reinforced thermoset thick molding compound for composite power train applications such as valve covers and timing gear covers.Key features and benefits are:Ideal f.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2103-20 CR-SX Fiberglass Reinforced Thermoset BMC Premi-Glas® 2103-20 CR-SX is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regu.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2143-24 CR-SX-HT Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2200-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2200-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2200-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2204-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2204-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Good dimensional stability, inclu.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2204-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2205-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 3101-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-10 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 3101-22 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-22 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 3101-25 Polyester BMC Premi-Glas® 3101-25 is a 25% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL .. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 3200-30 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-30 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | XY Direction |
Premix Premi-Glas® 2103-10 CRSX Polyester BMC Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
13.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON AX02747 ABS LNP* STAT-KON* AX02747 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | TMA |
Vyncolit W5000 Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral filled. Excellent dimensional stability and very low coefficient of linear expansion and excellent chemical resistance at elevated temperatures in severa.. |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TC153 PA46 FR(17) Thermal conductive material, Flame Retardant, Heat Stabilized |
|||
CTE, linear, Transverse to Flow | 25.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
13.9 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |