Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
LNP Lubricomp® EFL-4036 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
FKuR Kunststoff Bio-Flex® S 6540 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D572 |
Haysite 44500 Vinyl Ester SMC, 30% Glass Reinforced The 44500 series sheet molding compound offers high strength and excellent resistance to corrosive agents. This compression molding grade is formulated with a vinyl ester resin system. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | |
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Europe-Africa-Middle East) LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183/A |
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, Conditioned Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA4/6 GF50 HS BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackUL File Number: E1573.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP WFB44 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WFB44 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Glass Bead. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Europe-Africa-Middle East) Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | dry; ISO 1183 |
DSM Stanyl® 46HF4550 PA46-GF50 50% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | dry; ISO 1183 |
DSM Stanyl® TC153 PA46 FR(17) Thermal conductive material, Flame Retardant, Heat Stabilized |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
DSM Stanyl® TW241F10 Nylon 46-50% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
Barlog Plastics KEBAFLOW HF130 LCP, 30% glass fiber reinforced LCP-GF30Information provided by BARLOG plastics GmbH. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon CP-498W Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Conditioned) Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines fl.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183/A |
Addiplast Addinyl A2H M30 Flame Retardant Nylon 66, 30% Mineral Filled Flame retardant, 30% mineral filled, with halogensInformation provided by Addiplast. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 51986R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater substrateAppearance: Red colo.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 51986RA020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the producti.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP JF006E PES (Europe-Africa-Middle East) LNP* Thermocomp* JF006E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KF006 POM (Europe-Africa-Middle East) LNP* THERMOCOMP* KF006 is a compound based on Acetal Copolymer resin containing Glass Fiber |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | |
LATI Latilub 80-15T G/30 PPS, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PBT GF30 FR-S 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame Retardant and Non-BloomingProcessing Method: Injection MoldingInformation provided by .. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PBT GF30 FR X 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame RetardantUL File Number: E157318TPCI# 1006011Information provided by TP Composites, In.. |