DSM Arnite® BM4 240 (PBT+PET)-MD20

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + PET, Mineral Filled
Manufacturer DSM Engineering Plastics
Trade Name Arnite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnite® BM4 240 (PBT+PET)-MD20.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Mineral Reinforced
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ISO 1183
Water Absorption 0.35 %
0.35 %
Sim. To ISO 62
Moisture Absorption 0.150 %
0.150 %
Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.017 cm/cm
0.017 in/in
Sim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
Sim. To ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ISO 527-1/-2
Elongation at Break 2.2 %
2.2 %
ISO 527-1/-2
Tensile Modulus 4.50 GPa
653 ksi
ISO 527-1/-2
Charpy Impact Unnotched 3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 195 °C
383 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10