DSM Akulon® K125 PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer DSM Engineering Plastics
Trade Name Akulon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Akulon® K125 PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low Viscosity
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
dry; ISO 1183
Water Absorption 9.5 %
9.5 %
Sim. To ISO 62
Moisture Absorption 2.50 %
2.50 %
Sim. To ISO 62
Viscosity Test 152 cm³/g
152 cm³/g
Viscosity Number; ISO 307, 1157, 1628
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3