Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer A. Schulman, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection temperatures and pressures and minimizes stress in molding.ApplicationPolypropylene PP 1329H-01 meets FDA Regulation 21 CFR 177.1250, for all food contact applications.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.902 g/cc
0.902 g/cc
ASTM D792
Melt Flow 17 - 23 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 - 23 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.065 GPa
154.5 ksi
ASTM D790
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Gardner Impact 13.6 J
10.0 ft-lb
Users viewing this material also viewed the following: