Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufGuard M™ GPP1001M-P-2986 Grey PP, Flame Retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer S&E Specialty Polymers
Trade Name TufGuard M™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufGuard M™ GPP1001M-P-2986 Grey PP, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: High impact resistant, non-blooming flame retardant polypropylene compound designed for UL94 V-0 injection molding applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 0.980 - 1.02 g/cc
0.980 - 1.02 g/cc
ASTM D792
Melt Flow 15.0 - 21.0 g/10 min
15.0 - 21.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 10.3 MPa
>= 1500 psi
ASTM D2863
Tensile Strength, Yield >= 25.5 MPa
>= 3700 psi
ASTM D638
Elongation at Break >= 50.0 %
>= 50.0 %
Ultimate; ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched >= 0.641 J/cm
>= 1.20 ft-lb/in
ASTM D256
Dart Drop Total Energy >= 6.41 J/cm
>= 0.0120 ft-lb/mil
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 186.7 °C
368.1 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
Oxygen Index >= 28.0 %
>= 28.0 %
ASTM D2863