SGL Carbon Group SIGRAFIL C® C30 T400 EPY Continuous Tow Carbon Fiber with 400k filaments, Epoxy Sizing

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer SGL Carbon Group
Trade Name SIGRAFIL C®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SGL Carbon Group SIGRAFIL C® C30 T400 EPY Continuous Tow Carbon Fiber with 400k filaments, Epoxy Sizing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SIGRAFIL C as continuous tow is ideal for waving, prepregging, filament winding, Carbon Fiber Reinforced Plastics (CFRP) components, advanced composites, multi-axial production, unidirectional tapes, extrusion, pultrusion and other conversion processing. Characteristic properties of SIGRAFIL C include high tensile strength, high modulus of elasticity coupled with high electrical conductivity and compatibility with a large variety of resins.Information provided by SGL Carbon Group
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Fiber Density
Filament Diameter 7.0 µm
7.0 µm
Mechanical Properties Metric English Comments
Tensile Strength at Break 3800 MPa
551000 psi
ASTM D3379-78
Elongation at Break 1.5 %
1.5 %
ASTM D3379-75
Modulus of Elasticity 240 GPa
34800 ksi
ASTM D3379-78
Electrical Properties Metric English Comments
Volume Resistivity 0.0016 ohm-cm
0.0016 ohm-cm
Descriptive Properties Value Comments
Carbon Content, wt % >95
Sizing Content, % by weight 1
Weight per unit length, g/m 25