Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Akulon® F-X9215 PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer DSM Engineering Plastics
Trade Name Akulon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Akulon® F-X9215 PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low/Medium Viscosity
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
dry; ISO 1183
Water Absorption 9.5 %
9.5 %
Sim. To ISO 62
Moisture Absorption 2.50 %
2.50 %
Sim. To ISO 62
Viscosity Test 162 cm³/g
162 cm³/g
Viscosity Number; ISO 307, 1157, 1628
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
dry; ISO 527-1/-2
Elongation at Yield 8.0 %
8.0 %
dry; ISO 527-1/-2
Tensile Modulus 2.00 GPa
290 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
cond; ISO 179/1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
dry; ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
dry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
dry; ISO 11359-1/-2
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3