Material Notes:
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many specific potting and encapsulating applications such as modules, strain-sensitive components, transformers, and coils. All 2500 series systems exhibit excellent performance when exposed to adverse environments and temperature ranges between -55°C and +130°C.Cytec (Conap) EN-2543 Potting and Encapsulation AdhesiveSpecifically formulated to impart a flame resistance that will meet U.L. 94 V-O rating in 1/8" test sample.Passes Thermal Shock Test (10 Cycles, -65°C to 130°C)Non-Nutrient Fungus Resistance (MIL-STD-810B)Mix Ratio: 15/100 (by Weight)
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
Cured
Water Absorption 0.11 %
0.11 %
24 hours
Water Absorption at Saturation 0.0042 %
0.0042 %
30 Days
Viscosity 4750 cP

@Temperature 25.0 °C
4750 cP

@Temperature 77.0 °F
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Hardness, Shore D 45 - 55
45 - 55
Tensile Strength, Ultimate 8.62 MPa
1250 psi
Elongation at Break 50 %
50 %
Thermal Properties Metric English Comments
CTE, linear 140 µm/m-°C

@Temperature 20.0 °C
77.8 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.305 W/m-K
2.12 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 1.70e+14 ohm-cm
<= 1.70e+14 ohm-cm
Surface Resistance 8.90e+14 ohm
8.90e+14 ohm
Dielectric Constant 4.5

@Frequency 1000 Hz
4.5

@Frequency 1000 Hz
Dielectric Strength 25.6 kV/mm

@Thickness 1.59 mm
650 kV/in

@Thickness 0.0625 in
Dissipation Factor 0.075

@Frequency 1000 Hz
0.075

@Frequency 1000 Hz
Arc Resistance >= 120 sec
>= 120 sec
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 100 °C
4.00 hour

@Temperature 212 °F
360 min

@Temperature 60.0 °C
6.00 hour

@Temperature 140 °F
10080 min

@Temperature 25.0 °C
168.0 hour

@Temperature 77.0 °F
Pot Life 30.0 - 35.0 min

@Temperature 25.0 °C
30.0 - 35.0 min

@Temperature 77.0 °F
1 lbm
Descriptive Properties Value Comments
Color Tan or Black