Polymer Property : Pot Life = 35.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 30.0 - 35.0 min

@Temperature 25.0 °C
30.0 - 35.0 min

@Temperature 77.0 °F
1 lbm
Cytec EN-2543 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..