Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 8.90e+14 ohm | 8.90e+14 ohm | |
Cytec EN-2543 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Surface Resistance | 8.90e+14 ohm | 8.90e+14 ohm | Condition A; IPC TM-650 2.5.17.1 |
Arlon 25FR Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |