Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 4750 cP @Temperature 25.0 °C |
4750 cP @Temperature 77.0 °F |
|
Cytec EN-2543 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |