Mechanical Properties Metric English Comments
Izod Impact, Notched 0.250 J/cm

@Temperature -30.0 °C
0.468 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® DMX9254 PC
Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl..
Izod Impact, Notched 0.250 J/cm

@Temperature -30.0 °C
0.468 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® DMX9254 PC (Asia Pacific)
Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl..
Izod Impact, Notched 0.250 J/cm

@Temperature -30.0 °C
0.468 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® DMX9254 PC (Europe-Africa-Middle East)
Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl..
Izod Impact, Notched 0.250 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
0.468 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)
Information provided by Solvay Specialty Polymers.
Izod Impact, Notched 0.250 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
0.468 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec..
Izod Impact, Notched 0.250 J/cm

@Temperature 0.000 °C
0.468 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTAPROP 1000 V2 H Flame Retardant Polypropylene
PP homopolymerFlame retardant class V2, PBDE free, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.250 J/cm

@Temperature 0.000 °C
0.468 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTAPROP 1040 V2 K Flame Retardant Polypropylene
PP copolymerFlame retardant class V2, halogen free, good mechanical characteristicsInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.250 J/cm

@Temperature 23.0 °C
0.468 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTAPROP 1050 V0 HF H Flame Retardant Polypropylene
PP homopolymerFlame retardant class V0, halogen free, excellent mechanical characteristics, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.250 J/cm

@Temperature 0.000 °C
0.468 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTAPROP H 0360 T8 Polypropylene, 30% Mineral Filled
PP homopolymer 30% mineral fillerExtrusion gradeInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.250 J/cm

@Temperature 0.000 °C
0.468 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTAPROP H 10100 BS Polypropylene, 50% Mineral Filled
PP homopolymer 50% mineral fillerExcellent surface appearance, high densityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.250 J/cm

@Temperature 0.000 °C
0.468 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTAPROP H 1080 T6 T D Polypropylene, 40% Mineral Filled
PP homopolymer 40% mineral fillerGood physical and mechanical characteristics, high thermal stability, detergent resistanceInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.250 J/cm

@Temperature 0.000 °C
0.468 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTAPROP H 2550 CBS/E Polypropylene, 25% Mineral Filled
PP homopolymer 25% mineral fillerHigh gloss, very high melt flow rate, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.250 J/cm

@Temperature 0.000 °C
0.468 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTAPROP H 2560 C Polypropylene, 30% Mineral Filled
PP homopolymer 30% mineral fillerExcellent processability, good surface appearanceInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.250 J/cm

@Temperature 0.000 °C
0.468 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTAPROP HK 2540 T8 Polypropylene, 20% Mineral Filled
PP homo/copolymer 20% mineral fillerGood physical and mechanical propertiesInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.250 J/cm

@Temperature -20.0 °C
0.468 ft-lb/in

@Temperature -4.00 °F
ASTM D 638
Cossa Polimeri ESTAPROP K 0200 V2 Flame Retardant Polypropylene
PP copolymer extrusion gradeFlame retardant class V2, PBDE free, good impact strengthInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.250 J/cm

@Temperature -20.0 °C
0.468 ft-lb/in

@Temperature -4.00 °F
ASTM D 638
Cossa Polimeri ESTAPROP K 1280 T8 Polypropylene, 40% Mineral Filled
PP copolymer 40% mineral fillerExcellent physical and mechanical characteristics, good surface appearanceInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.250 J/cm

@Temperature 0.000 °C
0.468 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTASAN SAN 0840 GF Styrene Acrylonitrile
SAN with 20% glass fiber reinforcementExcellent dimensional stability, good heat resistanceInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 0.250 J/cm

@Temperature -20.0 °C
0.468 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
Braskem CP 401 HC Injection Molding Polypropylene
Description: CP 401HC is a medium melt flow rate heterophasic copolymer, specially designed to achieve high stiffness/impact strength balance. This product offers good surface appearance and process..