Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ConocoPhillips 595 NC Open Gear Lube

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips 595 NC Open Gear Lube.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Open Gear Lube 595 NC is a black, viscous, semi-fluid product that can be applied via central pumping systems that utilize injectors and nozzles for spray or drip application. Open Gear Lube 595 NC does not contain chlorinated solvents. Open Gear Lube 595 NC is designed for the lubrication of open gears, racks and pinions, swing gears, booms and sticks contained on mine and quarry shovels, drag lines and related equipment. Open Gear Lube 595 NC will perform over a wide temperature range above 15°F. The product will form a tenacious film that contains adhesive, extreme pressure properties, lubricity, rust and corrosion inhibitors and solid phase lubricating additives to provide maximum performance. Moreover, the lubricant resists water wash off and corrosion. Open Gear Lube 595 NC is removable and cleanable from decks, ladders and operating areas with wiping rags and conventional solvents or cleaning chemicals. The product is not the conventional heavy, tacky type that is extremely difficult and costly for maintenance removal.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM D-1298
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
ASTM D-2596
Four Ball Wear 0.500 mm
0.0197 in
ASTM D-2296
Timken Test 20400 g
45.0 lb
ASTM D-2509
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -9.44 °C
15.0 °F
Flash Point >= 149 °C
>= 300 °F
Descriptive Properties Value Comments
Appearance Viscous, Semi-Fluid
Color Black
Cone Penetration 325
Undiluted, ASTM D217
Copper Corrosion 1B
ASTM D130
Diluent Content 8 wt. %
Rust Pass
ASTM D665 (24hrs at 60°C)
Ventmeter Max 600 psig
Lincoln VE-1 (at 40°F)
Copyright © lookpolymers.com All Rights Reserved