Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil 102 Mobilgrease EAL Mobilgrease EAL 101 and 102 are supreme performance greases designed specifically for applications which are environmentally sensitive. These products are biodegradable and virtually non-toxic greas.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil 222 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Timken Test | >= 20400 g | >= 45.0 lb | |
ExxonMobil CM-P Mobilgrease CM Series Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil Ronex MP Exxon RONEX MP is a premium quality multipurpose grease that can be used in a wide range of automotive and industrial applications. RONEX MP consists of a mineral oil base fluid thickened with a lit.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil 221 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil 223 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil Mobil Polyrex EP 2 Mobil Polyrex EP 2 is a shear-stable polyurea grease with excellent extreme-pressure (EP) and load-carrying characteristics. The proprietary polyurea thickener system exhibits excellent resistance t.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ConocoPhillips SUPER-STA NLGI No. 1 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Timken Test | 20400 g | 45.0 lb | |
ChevronTexaco 100 NC Open Gear Lubricant FeaturesChevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubri.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ChevronTexaco 800 NC Open Gear Lubricant FeaturesChevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubri.. |
|||
Timken Test | 20400 g | 45.0 lb | OK Load |
ChevronTexaco Sugartex® Heavy Texaco Sugartex delivers value through:Reliability — High lubricant film strength withstands heavy shock loads and provides protection under boundary lubrication to minimize wear rate and prevent f.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil 101 Mobilgrease EAL Mobilgrease EAL 101 and 102 are supreme performance greases designed specifically for applications which are environmentally sensitive. These products are biodegradable and virtually non-toxic greas.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil 102 Mobilgrease EAL Mobilgrease EAL 101 and 102 are supreme performance greases designed specifically for applications which are environmentally sensitive. These products are biodegradable and virtually non-toxic greas.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil 222 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil 222 Special Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil 223 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Timken Test | >= 20400 g | >= 45.0 lb | |
ExxonMobil CM-L Mobilgrease CM Series Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ.. |
|||
Timken Test | >= 20400 g | >= 45.0 lb | |
ExxonMobil CM-P Mobilgrease CM Series Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil Mobil Polyrex EP 2 Mobil Polyrex EP 2 is a shear-stable polyurea grease with excellent extreme-pressure (EP) and load-carrying characteristics. The proprietary polyurea thickener system exhibits excellent resistance t.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil Ronex MP Exxon RONEX MP is a premium quality multipurpose grease that can be used in a wide range of automotive and industrial applications. RONEX MP consists of a mineral oil base fluid thickened with a lit.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ConocoPhillips EP Conolith® Grease NLGI NO. 00 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Timken Test | 20400 g | 45.0 lb | ASTM D 2509 |
ConocoPhillips Gear Shield NC Open Gear Lubricant Description: Conoco Gear Shield NC is a black, viscous fluid designed to lubricate open gears. Gear Shield NC contains neither chlorinated solvents nor lead compounds. Gear Shield NC is designed to .. |
|||
Timken Test | 20400 g | 45.0 lb | |
ConocoPhillips Tacna® 2000 NLGI No. 1 Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and o.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ChevronTexaco Delo® Synthetic Grease SF FeaturesChevron Delo Synthetic Grease SF is a high performance grease specifically engineered for trailer wheel-ends operating in all conditions, even under the most extreme high and low temperature.. |
|||
Timken Test | 20400 g | 45.0 lb | OK Load |
ChevronTexaco Sugartex® Texaco Sugartex delivers value through:Reliability — High lubricant film strength withstands heavy shock loads and provides protection under boundary lubrication to minimize wear rate and prevent f.. |
|||
Timken Test | 20400 g | 45.0 lb | ASTM D-2509 |
ConocoPhillips 595 NC Open Gear Lube Description: Conoco Open Gear Lube 595 NC is a black, viscous, semi-fluid product that can be applied via central pumping systems that utilize injectors and nozzles for spray or drip application. Op.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil 461 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Timken Test | >= 20400 g | >= 45.0 lb | |
ExxonMobil CM-L Mobilgrease CM Series Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil Mobil 1 Synthetic Grease Mobil 1 Synthetic Grease is an NLGI No 2 high-performance grease which combines a synthetic base fluid with a lithium complex soap thickener. The thickener system provides a high dropping point, whi.. |
|||
Timken Test | 20400 g | 45.0 lb | |
ExxonMobil 461 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |