Material Notes:
CALIBRE® 300EP series resins are general purpose polycarbonate resins and can be supplied with a mold release package, a UV stabilizer package or both. CALIBRE 300EP resins exhibit an excellent physical property balance of heat resistance, transparency and impact strength. The CALIBRE 300EP resins have a UL-94 rating of V-2(1). In addition the high melt flow rate allows complex parts to be easily molded.The CALIBRE 300EP series resins are typically used for appliances, storage media housings, electrical components and lighting.Available Melt Flow Rate: 22.Associated products: CALIBRE 300EP: without a mold release and UV stabilization package CALIBRE 301EP: including a mold release package CALIBRE 302EP: including a UV stabilizer package CALIBRE 303EP: including a mold release and UV stabilizer package.(1) These numerical flame spread ratings are small scale test values and are not intended to reflect hazards presented by these or any other materials under actual fire conditions.Ignition resistant chemical additives increase resistance to burning from minor flame sources and permit properly manufactured end products to meet the requirements of certain flammability tests, but resins will burn rapidly under the right conditions of heat and oxygen feed.Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM Data
Melt Density 1.01 g/cc
0.0365 lb/in³
Melt density
Water Absorption 0.15 %
0.15 %
Moisture Absorption at Equilibrium 0.32 %
0.32 %
Humidity Absorption
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Melt Flow 22 g/10 min

@Load 1.20 kg,
Temperature 300 °C
22 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM Data
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
Tensile Strength, Ultimate 65.5 MPa
9500 psi
ASTM Data
Tensile Strength, Yield 62.1 MPa
9010 psi
ASTM Data
Elongation at Break 120 %
120 %
ASTM Data
Elongation at Yield 6.0 %
6.0 %
ISO Data
Tensile Modulus 2.34 GPa
339 ksi
ASTM Data
Izod Impact, Notched 7.47 J/cm
14.0 ft-lb/in
ASTM Data
Izod Impact, Unnotched NB
NB
ASTM Data
Charpy Impact Unnotched NB
NB
ISO Data
NB
NB
ISO Data, Low Temp
Charpy Impact, Notched 1.10 J/cm²
5.24 ft-lb/in²
ISO Data, Low Temp
7.00 J/cm²
33.3 ft-lb/in²
ISO Data
Tensile Impact Strength 378 kJ/m²
180 ft-lb/in²
ASTM Data
Impact Test 72.3 J

@Temperature 23.0 °C
53.3 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.4 µm/m-°C

@Temperature 20.0 °C
38.0 µin/in-°F

@Temperature 68.0 °F
ASTM data
Specific Heat Capacity 1.96 J/g-°C
0.468 BTU/lb-°F
Thermal Conductivity 0.207 W/m-K
1.44 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
259 °F
Unannealed; ASTM Data
Vicat Softening Point 152 °C
306 °F
Flammability, UL94 V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Oxygen Index 26 %
26 %
Optical Properties Metric English Comments
Haze 1.1 %
1.1 %
Transmission, Visible 89 %
89 %
Electrical Properties Metric English Comments
Electrical Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM Data
Dielectric Constant 2.93

@Frequency 60 Hz
2.93

@Frequency 60 Hz
ASTM Data
2.93

@Frequency 1e+6 Hz
2.93

@Frequency 1e+6 Hz
ASTM Data
Dielectric Strength 16.5 kV/mm
419 kV/in
Dissipation Factor 0.00050

@Frequency 60 Hz
0.00050

@Frequency 60 Hz
0.0017

@Frequency 1e+6 Hz
0.0017

@Frequency 1e+6 Hz
ASTM Data