Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 149 °C | 300 °F | coc; ASTM D92 |
Paratherm Corporation Paratherm™ MR Heat Transfer Fluid Description: Paratherm MR® is a mid-range heat transfer fluid. It is efficient across the temperature range, thermally stable and cost-effective. Non-aromatic and non-toxic, the fluid is safe to .. |
|||
Flash Point | >= 149 °C | >= 300 °F | COC; ASTM D92 |
Solvay ALKAMULS® PSML 20 Surfactant Description: Sorbitan ester ethoxylate with a HLB of 16.7. Oil in water emulsifier for mineral and vegetable oils in metalworking. Solubilizer, antistat and lubricant for textile industry.Chemical N.. |
|||
Flash Point | >= 149 °C | >= 300 °F | COC; ASTM D92 |
Solvay ALKAMULS® PSTO 20 Surfactant Description: Good emulsification characteristics, particularly in combination with high or low HLB surfactants to form W/O or O/W emulsions.Chemical Name: ETHOXYLATED SORBITAN TRIOLEATECAS: 9005-70-.. |
|||
Flash Point | 149 °C | 300 °F | ASTM D92 |
ExxonMobil Univolt N 61B Univolt N 61B is a transformer oil that provides cooling, insulating, arc quenching, and cleaning properties while meeting the requirements of an ASTM D 3487 Type II fluid. Univolt N 61B is a full.. |
|||
Flash Point | >= 149 °C | >= 300 °F | ASTM D92 |
Dow BETAFOAM™ 87100 MDI & PMDI Isocyanate BETAFOAM™ 87100 is a component used to make low density, all water blown rigid polyurethane foam.Information provided by Dow |
|||
Flash Point | >= 149 °C | >= 300 °F | ASTM D92 |
Dow BETAFOAM™ 87120 Polyether / Polyol Blend BETAFOAM™ 87120 is a component used to make low density, all water blown rigid polyurethane foam.Information provided by Dow |
|||
Flash Point | >= 149 °C | >= 300 °F | ASTM D92 |
Dow BETAFOAM™ 87124 Polyether / Polyol Blend BETAFOAM™ 87124 is a component used to make high-density, all-water blown rigid polyurethane foam.Information provided by Dow |
|||
Flash Point | >= 149 °C | >= 300 °F | ASTM D92 |
Dow BETAFOAM™ 87155 Polyether / Polyol Blend BETAFOAM™ 87155 is a component used to make high-density, all-water blown rigid polyurethane foam.Information provided by Dow |
|||
Flash Point | >= 149 °C | >= 300 °F | ASTM D92 |
Dow BETAFOAM™ 87156 Polyether / Polyol Blend BETAFOAM™ 87156 is a component used to make a rigid, all-water blown molded foam with excellent thermal stability.Information provided by Dow |
|||
Flash Point | 149 °C | 300 °F | ASTM D92 |
ExxonMobil Univolt N 61B Univolt N 61B is a transformer oil that provides cooling, insulating, arc quenching, and cleaning properties while meeting the requirements of an ASTM D 3487 Type II fluid. Univolt N 61B is a full.. |
|||
Flash Point | 149 °C | 300 °F | Dry Film; ASTM D93, DIN 51 755 |
Chesterton 775 Moisture Shield Description: Chesterton® 775 Moisture Shield is a moisture displacing, clear protective coating that protects parts and equipment from corrosion for months. Sprayed on bare metal, it leaves a lubri.. |
|||
Flash Point | 149 °C | 300 °F | COC; ASTM D92 |
ExxonMobil SpectraSyn™ 2B Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |
|||
Flash Point | 149 °C | 300 °F | ASTM D-92 |
ConocoPhillips Hydroclear® 6 Ultra-Clean Spindle Oil Description: Conoco Hydroclear Ultra-Clean Spindle fluids comprise blends of special base oils and additives specially formulated for use in applications where a lubricant combining the properties o.. |
|||
Flash Point | >= 149 °C | >= 300 °F | |
ConocoPhillips 595 NC Open Gear Lube Description: Conoco Open Gear Lube 595 NC is a black, viscous, semi-fluid product that can be applied via central pumping systems that utilize injectors and nozzles for spray or drip application. Op.. |